Characterization and Beneficiation of Low-grade Wolframite Ore from Rafin Gabas, Nasarawa State, Nigeria: Liberation Size Determination and Comparison of Magnetic and Air-float Separation Using X-Ray Fluorescence
Dada Emily Bola
Analytical Department, National Metallurgical Development Centre, Jos, Plateau state, Nigeria.
Benjamin Abu Emmanuel *
Department of Chemistry, Faculty of Sciences, Federal University of Health Sciences, Otukpo, Benue State, Nigeria.
Konto Roseline Alamza
Analytical Department, National Metallurgical Development Centre, Jos, Plateau state, Nigeria.
Temitope Emmanuel-Alonge
Analytical Department, National Metallurgical Development Centre, Jos, Plateau state, Nigeria.
Ogunjobi Olawale Ayodeji
Analytical Department, National Metallurgical Development Centre, Jos, Plateau state, Nigeria.
*Author to whom correspondence should be addressed.
Abstract
This study investigated low-grade wolframite ore from Rafin Gabas, Nasarawa State, Nigeria, to characterise mineral associations, estimate an operational liberation size, and compare two dry beneficiation methods based on tungsten concentration. Polished sections were examined by reflected-light microscopy, while crushed material was classified by sieve analysis. Ore fractions and separation products were analysed using energy-dispersive X-ray fluorescence (XRF). The polished sections showed wolframite intergrown with cassiterite and iron-bearing phases within a quartz–calcite matrix. Sieve data and fraction assays indicated a working liberation size of approximately 0.25 mm (−250 +180 µm). The crude ore contained 139,251.7 mg/kg tungsten (approximately 13.9 wt%). Air-float separation produced a concentrate containing 501,623.4 mg/kg tungsten (approximately 50.2 wt%), whereas dry magnetic separation produced a concentrate containing 625,365.8 mg/kg (approximately 62.5 wt%). Magnetic middlings and tailings contained 407,016.4 mg/kg (approximately 40.7 wt%) and 1,984.6 mg/kg (approximately 0.2 wt%) tungsten, respectively. Magnetic separation therefore yielded the higher reported concentrate grade in these laboratory tests. However, product mass yields and tungsten recoveries were not established, and the XRF results require independent quantitative validation. The findings provide a preliminary basis for investigating magnetic upgrading and possible re-treatment of middlings without establishing overall process recovery or reproducibility. Interpretation should therefore remain restricted to the reported laboratory analyses and products.
Keywords: Wolframite, beneficiation, liberation size, magnetic separation, air-float separation, X-ray fluorescence